The smoke chamber is subject to all the worst exposure that cement manufacturing can cause, such as alkali attack, build-ups, anchor corrosion and high temperatures (~1300°C).
Click to enlarge
Our refractory solutions are listed on the table below:
Area / Temperature (°C) | Processing Conditions | Monolithic solution | Brick solution | Energy Saving brick solution |
---|---|---|---|---|
Smoke Chamber 900- 1100°C | Mild Abrasion Chemical attack Build-up | HÖGANÄS CAST /GUN LC 50 AR Severe Conditions HÖGANÄS CAST LC 60 AR HÖGANÄS CAST LC 75 AR HÖGANÄS CAST/GUN LC S10 Insulation HÖGANÄS INSUL CC 1,5L | Alex Viking 33 Severe Conditions Alsic 500 Insulation HÖGANÄS INSUL M E/brick (S+N) HIPOR 450/brick (S+N) Super1100E Porosil 23 | Viking 330 Severe Conditions Alsic 500 Insulation Insulation 1: Porosil 23/brick Insulation 2: HÖGANÄS INSUL 450/brick HÖGANÄS INSUL M E/brick (TAD) Super 1100E/slab (TAD) |